Processing Properties Metric English Comments
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Polymer Resources ABS-FR1 ABS, Flame Retardant
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Mold Temperature 54.0 - 71.0 °C
129 - 160 °F
Cavity surface temp. at equilibrium
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 54.0 - 71.0 °C
129 - 160 °F
Cavity surface temp. at equilibrium
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
PolyOne Edgetek® SY-15GB/000 Polystyrene (PS), Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 49.0 - 71.0 °C
120 - 160 °F
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE  (discontinued **)
Data provided by PolyOne.
Mold Temperature 60.0 - 71.1 °C
140 - 160 °F
PolyOne Lubri-Tech™ AT-10GB/15KV Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledAramid Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
PolyOne Lubri-Tech™ AT-15GF/10T Acetal-Copolymer, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
PolyOne Edgetek® AT-30GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 60.0 - 71.1 °C
140 - 160 °F
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated &nb
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 60.0 - 71.1 °C
140 - 160 °F
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 40.6 - 71.1 °C
105 - 160 °F
Ravago Manufacturing Americas Hylac® FR74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Mold Temperature 54.0 - 71.0 °C
129 - 160 °F
Cavity surface temp. at equilibrium
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 54.0 - 71.0 °C
129 - 160 °F
Cavity surface temp. at equilibrium
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Mold Temperature 60.0 - 71.0 °C
140 - 160 °F
PolyOne Lubri-Tech™ ATH-000/02T Homopolymer - 2% PTFE  (discontinued **)
Data provided by PolyOne.
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-68/25/E/SD Polypropylene Copolymer, 25% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 38.0 - 71.0 °C
100 - 160 °F
Average value: 54.4 °C Grade Count:7
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
PolyOne Edgetek® AT-10GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation.