Momentive Performance Materials IGS3719-D1 Insulating Glass Sealant, Gray

Category Polymer , Adhesive , Thermoset , Filled/Reinforced Thermoset , Silicone , Silicone, RTV, Construction Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials IGS3719-D1 Insulating Glass Sealant, Gray.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Cure Method: Alkoxy (Neutral). Tack-free time 0.5 hr. Peel Strength 50 lb/in. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 37
37
ASTM D2240
Tensile Strength, Ultimate 2.10 MPa
305 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Cure time to 0.125 in. is 2 hours