Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Oxford Polymers ABS 20CCF-MP-BK ABS, 20% Carbon Fiber Reinforced
Conductive Carbon Fiber (20% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and extrusion/Injection Molding Additives: Release AgentsInformation provided by Oxford P..
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Polymer Resources ABS-GP1 General Purpose ABS
General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy
Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
Cavity mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
Cavity mold surface temperature at equilibrium conditions
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin
Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant
Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS).
Mold Temperature 35.0 - 71.1 °C
95.0 - 160 °F
RTP Company RTP 6091-55A BLACK Specialty Thermoplastic Elastomer, PA-6 bondable - manufactured with Santoprene™ TPV technology
Mold Temperature 35.0 - 71.1 °C
95.0 - 160 °F
RTP Company RTP 6091-85A BLACK Specialty Thermoplastic Elastomer, PA-6 bondable - manufactured with Santoprene™ TPV technology
Mold Temperature 40.6 - 71.1 °C
105 - 160 °F
Ravago Manufacturing Americas Hylac® FR74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® M-2149 Polypropylene Homopolymer, 30% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 37.8 - 71.1 °C
100 - 160 °F
Fiberfil® M-2450 Polypropylene Copolymer
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 10.0 - 71.1 °C
50.0 - 160 °F
LTL Color Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Nylon/ABS alloy with high ductility and excellent chemical resistanceAll information provided by LTL Color Compounders, Inc.
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 32.2 - 71.1 °C
90.0 - 160 °F
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
TPI Porene® ABS-AN450 Flame Retardant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Mold Temperature 37.8 - 71.1 °C
100 - 160 °F
RTP Company RTP 2899 X 106530 A Value-added Thermoplastic Polyolefin Elastomer, Nylon 6 Overmolding
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
LTL Color Compounds ColorFast® GPA100 ABS
High impact, high gloss injection molding ABS, HB-rated, FDAAll information provided by LTL Color Compounders, Inc.
Mold Temperature 54.4 - 71.1 °C
130 - 160 °F
PolyOne Lubri-Tech™ AT-25GB/5T-2S Acetal-Copolymer, Glass Bead Filled, PTFE/Silicone Lubricated  (discontinued
Description/Features:Glass Bead FilledPTFE/Silicone LubricatedInformation provided by PolyOne Corporation.