Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Omni Plastics OmniTuff™ HPP GRC20 Homopolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Network Polymers Kepital® F20-25 Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 23.0 °C |
1.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding 40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6 Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hysun™ 693 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ NL-20GF/05T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers PPC-220 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® J-1/CF/40 BK PA66 |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Techmer ES Electrafil® J-1/CF/40 NAT PA66 |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF33 FR-N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PEI CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® HIPS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NG1400S Nylon 66, 40% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PA2SP0004 Nylon 6 Alloy Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256A |
Braskem TR3020NT Random Copolymer Polypropylene Description: High flexural modulus, very good mold release. Applications: Suggested uses include extrusion, compression molding, thermoforming. Process: Compression Molding. This resin meets the req.. |