Polymer Property : Linear Mold Shrinkage = 0.0030 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Network Polymers SAN 278 Medium Blue Tint
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
With Flow; ISO 2577
Polykemi AB POLYblend 85FS GF10 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
0.125 in; ASTM D955
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (DAM)
Information provided by Ravago.
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM Data MD
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
Linear Mold Shrinkage 0.0030 - 0.0080 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0080 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 699 X 94678 SSC-63386 Acrylonitrile Butadiene Styrene (ABS), Phosphorescent Green
This material passes Mitsubishi and Toyota Glow Material Specifications for trunk latch release levers.
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
With Flow; ISO 2577
Polykemi AB POLYshine PBT D204 GF30 FR PBT, Glass Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 209G HS  Nylon 4/6 (PA 4/6) Glass Fiber 50% - Heat Stable  (discontinued **)
Glass Fiber 50% - Heat StableComments:Glass FiberHeat Stable(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Infor..
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 282G HS  Nylon 4/6 (PA 4/6) Carbon Fiber 15% - Heat Stable  (discontinued **
Carbon Fiber 15% - Heat StableComments:Carbon FiberHeat Stable(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Inf..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Lehmann & Voss LUVOCOM® 1-8181 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
KKPC Kuhmo HF 402 Flame Retarded General Purpose HIPS
Key features: Good mechanical balance, High Strength. Common Uses: Parts needing strength.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance b..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Ineos Styrenics Polystyrene 147F (NAFTA)
An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ..
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic
Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in ..
Linear Mold Shrinkage 0.0030 - 0.010 cm/cm

@Thickness 3.175 mm
0.0030 - 0.010 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
RTP Company ESD A 280 Nylon 6/6 (PA), Carbon Fiber - ESD Protection - Static Dissipative
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 1005 TFE 10 Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - PTFE Lubricated
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
Polyram PlusTek RA301G6 Nylon 6.6, 30% Glass Fiber
30% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Eastman DuraStar DS1900HF Polymer, Natural
Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur..
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D 955
Cossa Polimeri ESTADIENE 1030 V0 Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Linear Mold Shrinkage <= 0.0030 cm/cm
<= 0.0030 in/in
cured 72 hrs @ RT
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material
QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM Data; MD
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry)
Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6.
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap..
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
A. Schulman ComAlloy Aqualoy® 143 Polypropylene, Glass Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an..
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 1199 X 115085 B Polyethylene Terephthalate Glycol Modified (PETG), Carbon Nanotube - ESD Protection
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 4605 HI Syndiotactic Polystyrene (SPS), Glass Fiber - Impact Modified
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm

@Thickness 3.17 mm
0.0030 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP PA66 20 GF BLK Nylon 6/6 (PA), Value Product - Glass Fiber - Heat Stabilized
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Axiall SP-6235 Rigid PVC, Molding
Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall..