Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 24.8 MPa | 3600 psi | 2 in/min; ASTM D638 |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | 2 in/min; ASTM D638 |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | chs 2 in/min; ASTM D638 |
Network Polymers NPP 50-5052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Ravago Manufacturing Americas Echo® RPEHDW NAT (Injection) HDPE Available in North America Recycled Content: Yes Color: Natural Form: PelletsProcessing Method: Injection Molded Information provided by Entec |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Ravago Manufacturing Americas Echo® RPEHDW NAT HDPE Available in North AmericaDescription: Fractional Melt Recycled Content: Yes Color: Natural Form: Pellets Information provided by Ravago |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Petromont 1201 High Density Polyethylene Resin Petromont HDPE 1201 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as multi-purpose shipp.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A6DE3 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | 2 in/min; ASTM D638 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 24.8 - 31.0 MPa | 3600 - 4500 psi | ASTM D638 |
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
LyondellBasell Petrothene® LR686001 High Density Polyethylene ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D412 |
Teknor Apex Monprene® MP-2860M-CR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Teknor Apex Synres® SR 1209A Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Plastics Group Polifil® RMC-10 10% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | vs. rigid PVC; 15 s set time |
Elmer's Products Aron Alpha® 403TB Cyanoacrylate Adhesive (Industrial Krazy Glue™) Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ISO 527-2 |
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, .. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | vs. polycarbonate; 20 s set time |
Elmer's Products Aron Alpha® 453TB Cyanoacrylate Adhesive (Industrial Krazy Glue™) Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa.. |
|||
Tensile Strength at Break | 24.8 MPa | 3600 psi | ASTM D638 |
Chase Plastics CP Pryme® PE200-HD20M General Purpose High Density Polyethylene Information provided by Chase Plastics. |