LG Chemical LI951 Heat Resistant ASA

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LI951 Heat Resistant ASA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Maximum Moisture Content 0.010
0.010
Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 50.0 MPa

@Thickness 3.20 mm
7250 psi

@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 25 %

@Thickness 3.20 mm
25 %

@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 77.5 MPa

@Thickness 6.40 mm
11200 psi

@Thickness 0.252 in
15mm/min; ASTM D790
Flexural Modulus 2.16 GPa

@Thickness 6.40 mm
313 ksi

@Thickness 0.252 in
15mm/min; ASTM D790
Izod Impact, Notched 1.08 J/cm

@Thickness 6.50 mm,
Temperature 23.0 °C
2.02 ft-lb/in

@Thickness 0.256 in,
Temperature 73.4 °F
ASTM D256
1.18 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.20 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C

@Thickness 6.40 mm
219 °F

@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 104 °C

@Load 5.00 kg
219 °F

@Load 11.0 lb
50°C/h; ASTM D1525
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Rear Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Middle Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
Front Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
Nozzle Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
Melt Temperature 210 - 240 °C
410 - 464 °F
Injection Molding
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Injection Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
Back Pressure 68.6 - 88.3 MPa
9950 - 12800 psi
Injection Molding
Screw Speed <= 80 rpm
<= 80 rpm
Injection Molding