Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C...
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Polykemi AB POLYfill PPC T4030 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant
Information provided by Polykemi AB
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Polykemi AB POLYfill PPH T2020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Polykemi AB POLYfill PP TOUCH 25325 R3 Polypropylene, Glass Fiber Reinforced, Scratch Resistant
Information provided by Polykemi AB
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
LG Chemical AF342 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Start Point: 60°C
Kingfa MAC-451 PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel..
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
LG Chemical EF-378 ABS, Flame Retardant, Halogen Free
Information Provided by LG Chem
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Injection Molding
LG Chemical HIPS 65IHE PS, Impact Modified
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
LG Chemical LUPOL HI5302A PP+MF15%, High Impact
Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
A temperature exceeding 80 °C (175 °F) should be avoided
Kraiburg TPE THERMOLAST® K TC7PAZ Thermoplastic Elastomer, Adhesion to PA
The AD/PA Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design elements..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Kraiburg TPE THERMOLAST® TP7NLB Thermoplastic Elastomer, Adhesion to SAN, ASA, PMMA
Typical Markets / Application Sectors:Industrial AppliancesElectrics & ElectronicsConsumer ElectronicsApplication Examples:SealsCoveringsDesign and functional elementsHandlesFunctional elementsAir i..
Mold Temperature 40.0 - 90.0 °C
104 - 194 °F
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
LG Chemical TR-558A ABS, Transparent, High Strength
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
LATI Latigray 47/1-01 CX/45 PP Copolymer
Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Supreme Petrochem SH 400 M High Impact Polystyrene
Characteristics High gloss Easy flow Processing MoldingApplications Air conditioner and cooler grills, refrigerator components Toys, use and throw camera, household articles Ball pen barrels, nov..
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Clariant Renol ABNN732017 Nylon 6 with anchored silicone
Data provided by Clariant Masterbatches
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
E-Polymers TEKAMID® TB110HI , High Impact PA6, DAM
High Impact resistance at low temperatureInformation provided by E-Polymers Co. Ltd.
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Eurotec® Tecotek® BC40 UF45 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, easy flow grade
Information provided by Eurotec®
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Ejection temperature
BASF Ultradur B 2550 PBT
Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in..
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
DAM; Injection Molding
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Kraiburg TPE THERMOLAST® K TC3PAN Thermoplastic Elastomer, Adhesion to PA  (Unverified Data**)
Typical Markets / Application Sectors:Electrical ToolsAutomotive InteriorAutomotive UndercarApplication Examples:HandlesSealsDesign and functional elementsVibration damping elementsAir inlet pipingS..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Kraiburg TPE THERMOLAST® K TC4PAN Thermoplastic Elastomer, Adhesion to PA  (Unverified Data**)
Typical Markets / Application Sectors:Electrical ToolsAutomotive InteriorAutomotive UndercarApplication Examples:HandlesSealsDesign and functional elementsVibration damping elementsAir inlet pipingS..
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Molding
LG Chemical LUPOL GP2300 PP+GF30%
Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical