Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Melt Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Melt Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Melt Temperature 210 - 260 °C
410 - 500 °F
Injection Molding
Polimeri Europa Edistir R 540E Polystyrene
HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection moldings. Designation: Thermoplastics IS..
Melt Temperature 210 - 240 °C
410 - 464 °F
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Melt Temperature 210 - 238 °C
410 - 460 °F
Polymer Resources ABS-G30 ABS, 30% Glass Reinforced
Acrylonitrile Butadiene Styrene, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Melt Temperature 210 - 288 °C
410 - 550 °F
RTP Company RTP 3399 X 117884 E Polyvinylidene Fluoride (PVDF), Carbon Nanotube - Electrically Conductive
Melt Temperature 210 °C
410 °F
Extrusion
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Melt Temperature 210 - 249 °C
410 - 480 °F
RTP Company RTP 405 HI Polystyrene (PS), High Impact - Glass Fiber
Melt Temperature 210 - 220 °C
410 - 428 °F
Injection Molding
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov..
Melt Temperature >= 210 °C
>= 410 °F
LyondellBasell Plexar® PX5335 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..
Melt Temperature >= 210 °C
>= 410 °F
LyondellBasell Plexar® PX5400 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..
Melt Temperature 210 - 250 °C
410 - 482 °F
Injection Molding
LG Chemical LI942 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical
Melt Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
Melt Temperature 210 - 230 °C
410 - 446 °F
LATI Latilub 82-05GR G/30 PA12, 30% Glass Fiber Reinforced, Graphite Filled
Self-lubricating product based on Polyamide 12 (PA12). Graphite. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Melt Temperature 210 - 260 °C
410 - 500 °F
Borealis BJ380MO Polypropylene Copolymer
BJ380MO is a very high melt flow heterophasic copolymer with high/medium impact strength and stiffness. This grade is designed for high-speed injection molding and contains nucleating and antistatic..
Melt Temperature 210 - 230 °C
410 - 446 °F
Borealis Borcoat™ BA213E Polypropylene for Steel Pipe Coating
Borcoat™ BA213E is a polypropylene compound used as a component in thermal insulation coating systems. Applications: Borcoat™ BA213E is recommended as a polymer to make foam for thermal insulatio..
Melt Temperature 210 - 230 °C
410 - 446 °F
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according..
Melt Temperature 210 - 250 °C
410 - 482 °F
Borealis HJ320MO Polypropylene
HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is ..
Melt Temperature 210 - 275 °C
410 - 527 °F
Borealis MG9641S Polyethylene
MG9641S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Melt Temperature 210 - 260 °C
410 - 500 °F
Borealis RE420MO Polypropylene Random Copolymer, Transparent
RE420MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is intended for injection molding and stretch blow molding. and is designed ..
Melt Temperature 210 - 230 °C
410 - 446 °F
Covestro Desmopan® DP 2590A Polyurethane
Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationBlown filmsPreprocessingMax. Water content..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Melt Temperature 210 - 270 °C
410 - 518 °F
Celanese Celstran® +PP-GF30-04CN02/10 PP, 30% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Melt Temperature 210 - 250 °C
410 - 482 °F
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp..
Melt Temperature 210 °C
410 °F
Extrusion
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Melt Temperature 210 - 220 °C
410 - 428 °F
Injection Molding
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
Melt Temperature 210 - 260 °C
410 - 500 °F
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled
Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good ..
Melt Temperature 210 - 277 °C
410 - 530 °F
RTP Company RTP 3399 X 117884 D Polyvinylidene Fluoride (PVDF), Carbon Nanotube - Electrically Conductive