Processing Properties Metric English Comments
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
PolyOne Stat-Tech™ PC-CB2/000 CR Polycarbonate (PC)
Stat-Tech™ PC-CB2/000 CR XP100827Information provided by PolyOne
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66)
Information provided by PolyOne
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Dry Time 3.00 hour
3.00 hour
Celanese Celcon® GC20 POM, 20% Glass Reinforced  (Unverified Data**)
Celcon® GC20 is a glass coupled formulation containing 20% fiber glass reinforcement to improve strength and stiffness.20% glass fiber, has been replaced with Hostaform® C 9021 GV1/20Information p..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® C 27021 XAP² ™ POM  (Unverified Data**)
PolyacetalcopolymerLow EmissionInformation provided by Celanese
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Extrusion Molding
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical KEYFLEX BT 5035D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection and Extrusion Molding
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Extrusion Molding
LG Chemical SH610S ABS, Excellent Surface, High Impact
Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUSEP SP2306F SPS+GF30%, Flame Retardant
Feature: Injection Molding, sPS+GF30%, Flame RetardantApplication: Pump Units, Pick-up Lends Holder, etcCAS No. 9003-53-6, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical
Dry Time 3.00 hour

@Temperature 50.0 °C
3.00 hour

@Temperature 122 °F
Cossa Polimeri ESTABIO PL 0560 T10 Biodegradable Plastic
Biodegradable plastic for the extrusion of disposablesCertified for food contactInformation provided by Cossa Polimeri S.r.l.
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural
Information provided by Eurotec®
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Celstran® PPS-CF30-01 PPS, 30% Specialty
Celstran PPS-CF30-01 is a 30% long carbon fiber reinforced polyphenylene sulfide. This material imparts excellent impact and extremlely high modulus properties that exceed that od short carbon fiber..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® C 9021 K POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® LW90BSX POM, Tribological
Hostaform« LW90BSX is a specialty low wear grade of acetal copolymer designed for a wide range of tribological applications, including POM/POM pairings. This grade's low wear system includes silic..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Celstran® PPS-GF30-01 PPS, 30% Glass Reinforced
30% long strand fiber glass reinforced polyphenylene sulfide30% long strand glass fiber reinforced polyphenylene sulfideInformation provided by Celanese
Dry Time 3.00 hour
3.00 hour
Celanese Celcon® CF802 POM, Specialty  (Unverified Data**)
Celcon® acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon® CF802 has been developed to dissipate static electricity from fuel handling systems...
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® MT12U03 POM, Medical Technology  (Unverified Data**)
Hostaform® MT12U03 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT12U03 is a moderately high flow grade for fa..
Dry Time 3.00 hour
3.00 hour
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetImpact modified, improved modulus and weld line, low emissionInformation provided by Celanese
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® C 52021 XAP POM, Unfilled
POM copolymerInformation provided by Celanese
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® C 9021 GV1/30 GT POM, 26% Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Dry Time 3.00 hour
3.00 hour
Celanese ZENITE ZE55201 LCP, 50% Mineral / Glass Reinforced
Zenite« ZE55201 is a 50% mineral/glass fiber reinforced liquid crystal polymer for injection molding. and It is specifically suitable for applications requiring ultra flatness.Information provided ..