Processing Properties Metric English Comments
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized
Nylon 6, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow
Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant
Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Dry Time 3.00 hour
3.00 hour
Celanese Celcon® M90UV POM, UV Resistant  (Unverified Data**)
Celcon® M90UV is an acetal copolymer developed as a natural UV light stabilized standard flow grade for overall performance in most molding applications. It has been formulated as a natural acetal ..
Dry Time 3.00 hour
3.00 hour
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced  (Unverified Data**)
Zenite 7244 is a 40% glass mineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Blow Molding
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical HIPS 410AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Extrusion Molding
LG Chemical KEYFLEX BT 1047D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical Lupox® GP1000SB PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
LG Chemical LUPOY GP2102 PC+GF10%
Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Extrusion Molding
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical LUPOL GP3400 PP+MF40%
Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica..
Dry Time 3.00 hour
3.00 hour
Extrusion
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese FORTRON CES50 PPS, 40% Specialty
Fortron CES50 is a 40% glass fiber reinforced material with a total chlorine content less than or equal to 900 ppm. It offers excellent physical properties similar to those of the Fortron 1140L6 pr..
Dry Time 3.00 hour
3.00 hour
Celanese Hostaform® S 9363 POM, Impact Modified
Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o..
Dry Time 3.00 hour
3.00 hour
Celanese Hostaform® M25AE POM, Unfilled
Hostaform« M25AE is a special grade of acetal copolymer targeted for extrusion shapes (rod, bar, plate, etc) free of center porosity in large diameters and thicknesses.Information provided by Celan..
Dry Time 3.00 hour
3.00 hour
Celanese Celcon® GC15 POM, 15% Glass Reinforced  (Unverified Data**)
Celcon® GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.15% glass fibers, coupled for improved stiffnessStandard reciprocating sc..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® C 9021 GV1/20 POM, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 20 % glass fibersInformation provided by Celanese
Dry Time 3.00 hour
3.00 hour
Celanese Hostaform® CF802 10/9022 POM, Specialty
Hostaform« acetal copolymer grade CF802 10/9022 is a conductive, fuel compatible general purpose acetal copolymer. Hostaform« CF802 10/9022 has been developed to dissipate static electricity from ..
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Celanese Hostaform® LX90GC15 POM, 15% Specialty
Preliminary Data SheetInformation provided by Celanese
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
LG Chemical KEYFLEX TO1075AR Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical
Dry Time 3.00 hour
3.00 hour
Celanese ZENITE ZE55201 LCP, 50% Mineral / Glass Reinforced
Zenite« ZE55201 is a 50% mineral/glass fiber reinforced liquid crystal polymer for injection molding. and It is specifically suitable for applications requiring ultra flatness.Information provided ..
Copyright © lookpolymers.com All Rights Reserved