Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 210 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 210 - 240 °C
410 - 464 °F
Extrusion
Polimeri Europa Edistir N 1840 Polystyrene
General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm..
Melt Temperature 210 - 249 °C
410 - 480 °F
RTP Company RTP 400 HI Polystyrene (PS), High Impact
Melt Temperature 210 - 249 °C
410 - 480 °F
RTP Company RTP 400 HI UV Polystyrene (PS), High Impact - UV Stabilized
Melt Temperature 210 - 240 °C
410 - 464 °F
Extrusion
Polimeri Europa Edistir RCL 600 Polystyrene  (discontinued **)
Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets..
Melt Temperature 210 - 230 °C
410 - 446 °F
LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)  (discontinued **)
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Melt Temperature 210 - 240 °C
410 - 464 °F
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic  (discontinued **)
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Melt Temperature >= 210 °C
>= 410 °F
LyondellBasell Plexar® PX3216 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..
Melt Temperature 210 - 220 °C
410 - 428 °F
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Melt Temperature 210 - 240 °C
410 - 464 °F
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Melt Temperature 210 - 240 °C
410 - 464 °F
Injection Molding
LG Chemical PT270 ABS
Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical
Melt Temperature 210 °C
410 °F
LCL-PR29
Intercontinental Polymers CoPET 214-02 CoPET Polymer Type - Clear, Low Melt Polyester Pellets
Applications: Low MeltInformation provided by Intercontinental Polymers.
Melt Temperature 210 - 240 °C
410 - 464 °F
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Melt Temperature 210 - 240 °C
410 - 464 °F
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Melt Temperature 210 - 240 °C
410 - 464 °F
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Melt Temperature 210 °C
410 °F
Teknor Apex Chemlon® 267 Nylon 6, Impact Modified
Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good ..
Melt Temperature 210 - 230 °C
410 - 446 °F
Borealis Borcoat™ BA213E Polypropylene for Steel Pipe Coating
Borcoat™ BA213E is a polypropylene compound used as a component in thermal insulation coating systems. Applications: Borcoat™ BA213E is recommended as a polymer to make foam for thermal insulatio..
Melt Temperature 210 - 225 °C
410 - 437 °F
Molding
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 210 - 250 °C
410 - 482 °F
Borealis HJ320MO Polypropylene
HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is ..
Melt Temperature 210 - 275 °C
410 - 527 °F
Borealis MG9647B Polyethylene
MG9647B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
Melt Temperature 210 - 238 °C
410 - 460 °F
RTP Company RTP 1502-65D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber
Melt Temperature 210 - 260 °C
410 - 500 °F
Borealis Bormod™ BE961MO Polypropylene for Injection Molding
Bormod BE961MO is an heterophasic copolymer characterized by an optimum combination of high stiffness, low creep and very high impact strength.Bormod BE961MO is a new generation grade for very fast ..
Melt Temperature 210 - 249 °C
410 - 480 °F
RTP Company ESD 482 HI Polystyrene (PS); Carbon Fiber - Impact Modified - Electrically Conductive
Melt Temperature 210 - 230 °C
410 - 446 °F
Covestro Desmopan® DP 9395AU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationPneumatic hosesProfilesCable sheathingsInject..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Melt Temperature 210 - 260 °C
410 - 500 °F
Carmel Olefins CAPILENE® QU 73 AV Propylene Random Copolymer
Description: CAPILENE® QU 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QU 73 AV is clarified with antista..
Melt Temperature 210 - 220 °C
410 - 428 °F
Injection Molding
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform..
Melt Temperature 210 - 260 °C
410 - 500 °F
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance..
Melt Temperature 210 - 220 °C
410 - 428 °F
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer.
Melt Temperature 210 - 220 °C
410 - 428 °F
Injection Molding
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t..
Melt Temperature 210 - 220 °C
410 - 428 °F
Injection Molding
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the..
Copyright © lookpolymers.com All Rights Reserved