Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 235°C |
Kingfa HR-527B Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Front Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 235°C |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LI951 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical |
|||
Front Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC3CSN Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC3GPZ Thermoplastic Elastomer, General purpose The GP/FG Series is recommended for a variety of different applications. It is particularly appropriate for passenger compartments. The compounds are available in natural and black colors. Typical a.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC4CSZ Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC5TPN Thermoplastic Elastomer, General Purpose, Technical Performance The GP/AP Series is recommended for technical applications with excellent adhesion to PP. The compounds are available in natural and black colors. Typical applications:Function and design elements H.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC5TPZ Thermoplastic Elastomer, General Purpose, Technical Performance The GP/AP Series is recommended for technical applications with excellent adhesion to PP. The compounds are available in natural and black colors. Typical applications:Function and design elements H.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC6CSN Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TC7FLN Thermoplastic Elastomer, Flame retardant The FR/AP Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Automo.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TF5CGN Thermoplastic Elastomer, Natural The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical appl.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TF6THT Thermoplastic Elastomer, high transparency The FC/ht Series is a highly transparent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP. Typical applications:.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TF7CGN Thermoplastic Elastomer, Natural The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical appl.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TF7CGT Thermoplastic Elastomer, Translucent The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical appl.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TP7LDZ Thermoplastic Elastomer, Low Density, Automotive Exterior Applications The UV/LD/b Series is recommended for applications requiring high UV resistance. It is particularly appropriate for automotive exterior. Typical applications: Cowls gasketsRoof rimsWater deflectorsW.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® M TM3MHD Thermoplastic Elastomer, for medical and pharmaceutical technology The MC/n Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The compounds are produced exclusively by a special med.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® M TM7MED Thermoplastic Elastomer, for medical and pharmaceutical technology The MC/tl Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The compounds are produced exclusively by a special me.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TC0LEZ Thermoplastic Elastomer, UV resistance The UV/FG Series is recommended for applications requiring high UV resistance. It is particularly appropriate for automotive exterior and interior components. Typical applications: Cowls gasketsRoof.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC7CSN Thermoplastic Elastomer, Optimized compression set The CS Series is recommended for sealing applications, providing an excellent compression set. The compounds are available in natural and black colors. Typical applications: FasteningsGrommetsMembra.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TF6AAF Thermoplastic Elastomer, Transparent The FC/HE/tl Series is recommended for applications with food contact, providing excellent resilience properties. The series is available in translucent colors. Typical applications: Closures Flexib.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® M TM6MHD Thermoplastic Elastomer, for medical and pharmaceutical technology The MC/n Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The compounds are produced exclusively by a special med.. |
|||
Front Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Extrusion |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Extrusion |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Extrusion |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TC8FLN Thermoplastic Elastomer, Flame retardant The FR/AP Series is recommended for applications requiring high flame retardance. The compounds are halogen free and available in natural and black colors. Typical applications: Cable holders Automo.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | Injection |
Kraiburg TPE THERMOLAST® K TC9TPZ Thermoplastic Elastomer, General Purpose, Technical Performance The GP/AP Series is recommended for technical applications with excellent adhesion to PP. The compounds are available in natural and black colors. Typical applications:Function and design elements H.. |
|||
Front Barrel Temperature | 220 °C | 428 °F | |
Kraiburg TPE THERMOLAST® K TF9CGN Thermoplastic Elastomer, Natural The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical appl.. |