Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 6.40 mm |
11200 psi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical LI951 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 77.5 MPa | 11200 psi | ASTM D790 |
Cheng Yu Plastic 3265 TPE Rubber |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |