Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 220 °C | 428 °F | |
Multibase TPSiV™ 3011-85A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 65-8347/RD PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 245 °C | 428 - 473 °F | Injection |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Nozzle Temperature | 220 °C | 428 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | |
Lavergne VYSTYRENE PS 3901 High Impact Polystyrene Vystyrene PS 3901 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem AB845EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem AB855LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem AB860EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem GP-945 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem LP-845 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem LP-855 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 240 °C | 428 - 464 °F | |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection Molding |
Stellarchem 475-845N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 220 - 235 °C | 428 - 455 °F | |
Lubrizol Estane® S368D Thermoplastic Polyurethane Type: Estane® S368D is a Shore 68D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Nozzle Temperature | 220 - 230 °C | 428 - 446 °F | Injection |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Nozzle Temperature | 220 - 250 °C | 428 - 482 °F | |
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |