Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Mold Temperature | 27.0 - 60.0 °C | 80.6 - 140 °F | |
Eastman Eastalloy MA510 Polymer
(discontinued **) Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhan.. |
|||
Mold Temperature | 15.0 - 60.0 °C | 59.0 - 140 °F | |
SABIC M200024 Linear Low Density Polyethylene for Injection Molding Product Description: M200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give good f.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa FRHIPS-980 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | Start Point: 50°C |
Kingfa HF-626 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | A temperature exceeding 80 °C (175 °F) should be avoided |
Kraiburg TPE COPEC® CC6FDN Thermoplastic Elastomer, adhesion to ABS, PC and PC/ABS The VS/MR/AD1 Series is recommended for applications in the consumer electronics section. The series features an exceptionally silky and velvety surface, accompanied by an outstanding resistance to .. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Kraiburg TPE HIPEX® HX6ICN Thermoplastic Elastomer, High Performance The HTR/OR Series is recommended for applications requiring high temperature and oil resistance. Typical applications: ClosuresFasteningsFlexible ConnectionsSealsMaterial advantages: Excellent heat .. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Kraiburg TPE HIPEX® HX8ICZ Thermoplastic Elastomer, High Performance The HTR/OR Series is recommended for applications requiring high temperature and oil resistance. Typical applications: ClosuresFasteningsFlexible ConnectionsSealsMaterial advantages: Excellent heat .. |
|||
Mold Temperature | 26.7 - 60.0 °C | 80.0 - 140 °F | function of wall thickness |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Solvay TECHNYL® C 230 PA6, DRY Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibili.. |
|||
Mold Temperature | 10.0 - 60.0 °C | 50.0 - 140 °F | ISO 294 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Supreme Petrochem SC 201E General Purpose Polystyrene CharacteristicsVery high molecular weight High heat grade Good melt strength Good clarity and mechanical strengthProcessing Extrusion MoldingApplicationsExtruded embossed sheets, OPS, foamed meat t.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Supreme Petrochem SC 208 General Purpose Polystyrene CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a .. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Injection Molding |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Injection Molding |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
TPI Porene® GA300 High Flow Grade, High Gloss ABS INJECTION MOLDING. APPLIANCES, BUSINESS EQUIPMENT, ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Inform.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Injection Molding |
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Mold Temperature | 30.0 - 60.0 °C | 86.0 - 140 °F | |
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear.. |
|||
Mold Temperature | 16.0 - 60.0 °C | 60.8 - 140 °F | |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Mold Temperature | 26.7 - 60.0 °C | 80.0 - 140 °F | |
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Higher mold temperature provides a product with excellent surface finishing and less residual stress. |
Diamond Polymers ABS 3501 GF-10 Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Higher mold temperature provides a product with excellent surface finishing and less residual stress. |
Diamond Polymers ABS 3502E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
E-Polymers TEKAMID® TB120L NCR , High Crystallinity PA6, DAM Precise injection, high crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Mold Temperature | 25.0 - 60.0 °C | 77.0 - 140 °F | |
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11 Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Plastcom SLOVALEN PH 91 GF 15 Polypropylene Homopolymer, 15% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 15% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | |
Kraiburg TPE THERMOLAST® K TF5ADG Thermoplastic Elastomer, General purpose, adhesion to PC, ABS, PC/ABS
( Application Examples:Soft touchHandlesConsumer articlesMaterial Advantages:For co molded parts without patent infringementEasy to colorEasy to processExcellent adhesion in coinjection molding (depen.. |
|||
Mold Temperature | 37.8 - 60.0 °C | 100 - 140 °F | |
RTP Company RTP 1205-70D TFE 20 Polyurethane Thermoplastic Elastomer (TPU) Glass Fiber 30% - PTFE 20% - 70 Shore D Glass Fiber 30% - PTFE 20% - 70 Shore DComments:Glass FiberPTFE Lubricated70-D DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect pro.. |