Polymer Property : Vicat Softening Point = 104 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 104 °C
219 °F
ISO 306/A50
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
Vicat Softening Point 104 °C
219 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific)
Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Ravago Manufacturing Americas Hybrid S493 ABS + Polycarbonate Alloy
Medium Impact, Enhanced Heat PerformanceEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin fa..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin
Excellent ESCR, Excellent toughness, High strength, High flexibilityApplications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkl..
Vicat Softening Point 104 °C
219 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 104 °C

@Load 1.00 kg
220 °F

@Load 2.20 lb
ASTM-D1525
Ineos ABS Lustran® ABS 349
Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives.
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Lushan L-5R Polyethylene Copolymer Adhesive for Steel Pipe Coating
Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro..
Vicat Softening Point 104 °C
219 °F
1000 g; ASTM D1525
LG Chemical 25SPE GPPS
Heat resistance, Chemical resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Superior extrusion pr..
Vicat Softening Point 104 °C
219 °F
(50 °C/h / 50N) - B/50; ISO 306
Styrolution Luran® S 778 T ASA
Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Vicat Softening Point 104 °C
219 °F
B/120; ISO R306
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Vicat Softening Point 104 °C
219 °F
B/120; ISO R306
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR
Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries.
Vicat Softening Point 104 °C

@Load 1.02 kg
219 °F

@Load 2.25 lb
Rate B (120°C/h); ASTM D1525
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp..
Vicat Softening Point 104 °C

@Load 5.10 kg
219 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution Absolan® 2150 SAN
Absolac 2150 Crystal is a heat and chemical resistant gradeInformation provided by Styrolution
Vicat Softening Point 104 °C
219 °F
ASTM D1525
American Polymers 370 Polystyrene, High Heat
Data provided by American Polymers, Inc. A high heat polystyrene produced in pellet form. It has excellent strength and clarity as well as fast set-up properties. Used in the manufacture of toys,..
Vicat Softening Point 104 °C
219 °F
Conditioned 4 hours @ 70°C (158°F); ASTM D1525
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Vicat Softening Point 104 °C
219 °F
0.125 inch, 1 Kg; ASTM D1525
Diamond Polymers ABS 2512
Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc.
Vicat Softening Point 104 °C

@Load 1.00 kg
219 °F

@Load 2.20 lb
120°C/hr; ASTM D1525
Diamond Polymers Centrex® 810 Injection Molding Grade
Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and ..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Dow DOWLEX™ 2078G Linear Low Density Polyethylene
Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
Vicat Softening Point 104 °C

@Load 1.00 kg,
Thickness 3.17 mm
219 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers ASA S-170 Lt Grey 50283UV f1 ASA Weatherable Polymers Injection Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 104 °C
219 °F
Dow Tyril® 1011 SAN
TYRIL® 1011 SAN copolymer is a light stabilized general purpose injection molding resin available in crystone color only. It exhibits excellent weathering characteristics, high strength, good chemi..
Vicat Softening Point 104 °C
219 °F
50°C/hr; 50N; ASTM D1525
Arkema Group Plexiglas® V825 Acrylic
Plexiglas® V825 is a thermoplastic acrylic resin formulated for injection molding and extrusion applications. It is characterized by its high heat resistance and high melt flow. Plexiglas® V825 h..
Vicat Softening Point 104 °C
219 °F
50°C/hr; 50N; ASTM D1525
Arkema Group Plexiglas® V826 Acrylic
Plexiglas® V826 is a thermoplastic acrylic resin formulated for injection molding and extrusion applications. It is characterized by its excellent heat resistance and chemical resistance. Plexigla..
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Americas Styrenics EC6600 High Impact Polystyrene
Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy..
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B9086 (FDA Odor Mask), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 104 °C
219 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Vicat Softening Point 104 °C
219 °F
50B; ISO 306
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate
SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX ..