Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific) CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Thickness 3.17 mm |
0.0040 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers GPP-330 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0065 cm/cm | 0.0040 - 0.0065 in/in | |
LATI Latilub 52/30-15T G/30 PP Homopolymer, 30% Glass Fiber Reinforced Self-lubricating product based on Polypropylene homopolymer (PPh). PTFE. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Thickness 3.17 mm |
0.0040 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF/M40 HS L 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedTPCI# 7395102Informat.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Thickness 3.17 mm |
0.0040 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® POM CO GF25 CC 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 25% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® SV-0167 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | Dry |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Thickness 2.00 mm |
0.0040 in/in @Thickness 0.0787 in |
|
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | ISO 294-4 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Thickness 2.00 mm |
0.0040 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Diameter 2.00 mm |
0.0040 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 cm/cm @Diameter 2.00 mm |
0.0040 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |