Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific) Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1102A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | DIN 53452; ASTM D790 |
Kolon NOPLA® KE911 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
2.5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-20 Polycarbonate, General Purpose Features: Standard, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformation .. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-20MRA30 Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesIn.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-20UVR30 Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household ap.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-30 Polycarbonate, General Purpose Features: Standard, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications, Le.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-30FRT12 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-40MRA Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Kotec Carbotex K-50UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household application.. |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical TR300 MABS, Flame Retardant, Transparency Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch.. |
|||
Flexural Modulus | 2.16 GPa @Temperature 23.0 °C |
313 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene Applications:injection moldinghelmetsautomotive |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | ASTM D790 |
Hannam Chemical Hanalac 711 ABS, Plating Grade Plating grade with excellent moldability and easy to surface treat. It also has a strong adhesive strength after plating and an excellent heat cycle. Applications: Appliances, TV frames, automoti.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® HG-0760AT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced WNP GradeInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SR-0320 K ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | |
Zylog Hipolyene® 1535 T5 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.16 GPa | 313 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® X5402 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Flexural Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Modulus | 2.16 GPa @Thickness 6.40 mm |
313 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade High Flow, Medium ImpactInformation provided by Bhansali |