Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® BRZ 247 W PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BRZ 247 W PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibilityGood impact strength even at low temperatures Grilon BRZ 247 W is used typically for coextruded fuel lines, coolant pipes in deep freezer units, vulcanization mandrels, and vacuum lines.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 25.0 MPa
3630 psi
conditioned; ISO 2039-1
35.0 MPa
5080 psi
dry; ISO 2039-1
Tensile Stress 25.0 MPa

@Strain 50.0 %
3630 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
30.0 MPa

@Strain 50.0 %
4350 psi

@Strain 50.0 %
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.380 GPa
55.1 ksi
conditioned; ISO 527-1/-2
0.650 GPa
94.3 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
Melting Point 215 °C
419 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 29.0 kV/mm
737 kV/in
conditioned; IEC 60243-1
31.0 kV/mm
787 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Air intake sytems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Processing Other Extrusion
Product Attributes Flexible
Special Characteristics High impact or impact modified
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved