Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ASTM D696 |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 0.000 - 40.0 °C |
77.8 µin/in-°F @Temperature 32.0 - 104 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
1 |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 0.000 - 40.0 °C |
77.8 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 0.000 - 40.0 °C |
77.8 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 0.000 - 40.0 °C |
77.8 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 0.000 - 40.0 °C |
77.8 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 W 20 PA12 Product Description: Grilamid L 20 W 20 is a semi-flexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 is heat stabilized. The main features of Grilamid L 20.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 40 X PA12-I Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Covestro Texin® 270 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 22A W 40 X PA12-I Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 20 X PA12-I Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 40 ESD PA12 Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LKN-3H PA12-GB30 Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-2 |
Celanese RITEFLEX 672 TPC, Unfilled Riteflex 672 is a 72 Shore D Hardness thermoplastic polyester elastomer with a high modulus.Information provided by Celanese |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-2 |
Celanese RITEFLEX 677 TPC, Unfilled Riteflex 677 is a thermoplastic polyester elastomer with nominal hardness of 77 shore D and high modulus.Information provided by Celanese |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 23.0 - 250 °C |
77.8 µin/in-°F @Temperature 73.4 - 482 °F |
ASTM D696 |
Solvay Specialty Polymers Algoflon® 25CAR B PTFE; Carbon Filled
(discontinued **) Data provided by the manufacturer.25 wt.% Electrog. Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, .. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 23.0 - 250 °C |
77.8 µin/in-°F @Temperature 73.4 - 482 °F |
ASTM D696 |
Solvay Specialty Polymers Algoflon® 50 INOX PTFE; Stainless Steel Filled
(discontinued **) Data provided by the manufacturer.50 wt.% Stainless Steel. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, a.. |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C @Temperature 23.0 - 55.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® N2650 Z6 POM + PUR Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 140 µm/m-°C | 77.8 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® MT® SlideX™ 2404 POM, Medical Technology POM copolymerInformation provided by Celanese |