Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 25.0 MPa @Strain 1.00 %, Temperature 150 °C |
3630 psi @Strain 1.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 25.0 MPa @Strain 1.00 %, Temperature 150 °C |
3630 psi @Strain 1.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 25.0 MPa @Strain 2.00 %, Temperature 80.0 °C |
3630 psi @Strain 2.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 25.0 MPa @Strain 0.500 % |
3630 psi @Strain 0.500 % |
|
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Tensile Stress | 25.0 MPa @Strain 2.50 %, Temperature 0.000 °C |
3630 psi @Strain 2.50 %, Temperature 32.0 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 25.0 MPa @Strain 10.0 %, Temperature 80.0 °C |
3630 psi @Strain 10.0 %, Temperature 176 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 25.0 MPa @Strain 50.0 % |
3630 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril.. |
|||
Tensile Stress | 25.0 MPa @Strain 50.0 % |
3630 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Tensile Stress | 25.0 MPa @Strain 50.0 % |
3630 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Tensile Stress | 25.0 MPa @Strain 50.0 % |
3630 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
Tensile Stress | 25.0 MPa @Strain 50.0 % |
3630 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Tensile Stress | 25.0 MPa @Strain 1.17 %, Time 36000 sec |
3630 psi @Strain 1.17 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Tensile Stress | 25.0 MPa @Strain 1.34 %, Time 360000 sec |
3630 psi @Strain 1.34 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Tensile Stress | 25.0 MPa @Strain 2.03 %, Time 3.60e+6 sec |
3630 psi @Strain 2.03 %, Time 1000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal.. |
|||
Tensile Stress | 25.0 MPa @Strain 0.730 %, Time 360000 sec |
3630 psi @Strain 0.730 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 25.03 MPa @Strain 0.230 %, Temperature 40.0 °C |
3630 psi @Strain 0.230 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 25.0 MPa @Strain 0.500 %, Temperature 90.0 °C |
3630 psi @Strain 0.500 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Stress | 25.0 MPa @Strain 0.500 %, Temperature 60.0 °C |
3630 psi @Strain 0.500 %, Temperature 140 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Stress | 25.0 MPa @Strain 300 % |
3630 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 25.0 MPa @Strain 6.00 %, Temperature 140 °C |
3630 psi @Strain 6.00 %, Temperature 284 °F |
ISO 527 |
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | >= 25.0 MPa @Strain 100 % |
>= 3630 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 272D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 25.0 MPa @Strain 300 % |
>= 3630 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 495A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 25.0 MPa @Temperature 240 °C |
3630 psi @Temperature 464 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |
|||
Tensile Stress | 25.0 MPa @Temperature 200 °C |
3630 psi @Temperature 392 °F |
|
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |
|||
Tensile Stress | 25.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
3630 psi @Strain 1.00 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Tensile Stress | >= 25.0 MPa @Strain 100 % |
>= 3630 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 672D Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 25.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
3630 psi @Strain 1.00 %, Time 1000 hour |
100°C; DIN 50014-23/50-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |