Electrical Properties Metric English Comments
Dielectric Strength 31.0 - 49.0 kV/mm
787 - 1240 kV/in
Average value: 42.7 kV/mm Grade Count:3
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
Dielectric Strength 31.0 kV/mm
787 kV/in
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022..
Dielectric Strength 31.0 kV/mm
787 kV/in
Ineos ABS Lustran® H604
Standard impact strength.,Property data per ISO test methods.
Dielectric Strength 31.0 kV/mm
787 kV/in
DIN 53481
Kraiburg TPE THERMOLAST® K TC6CCT Transparent Cable Extrusion TPE
Transparent compound for cable extrusionSubstitute for PVC-P or siliconExtremely flexible materialFlexible in low temperaturesColoring in any shadeTypical Applications: Transmission cablesLoudspeake..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance
Dielectric Strength 31.0 kV/mm

@Thickness 1.00 mm
787 kV/in

@Thickness 0.0394 in
d.a.m.; IEC 60243-1
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant
PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS.
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243
Solvay TECHNYL® C 52G1 V20 PA6, DRY
Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer..
Dielectric Strength 31.0 kV/mm
787 kV/in
ASTM D149
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade
(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Covestro Makroblend® S 7916/2 Polycarbonate + PBT, Impact Grade
ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing..
Dielectric Strength 31.0 kV/mm
787 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® TSG-50 FA PA666-GF50
Information provided by EMS Grivory
Dielectric Strength 31.0 kV/mm
787 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® TSG-50 PA666-GF50
Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne..
Dielectric Strength 31.0 kV/mm
787 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI
Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesti..
Dielectric Strength 31.0 kV/mm
787 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50
Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Dielectric Strength 31.0 kV/mm
787 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40
Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Dielectric Strength 31.0 kV/mm
787 kV/in
DAM; IEC 60243-1
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers
Dielectric Strength 31.0 kV/mm
787 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® TR 90 UV PAMACM12
Product description: Grilamid TR 90 UV natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid 90 UV natural offers outstanding propert..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 243-1
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced
30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 243-1
Azoty Tarnow™ Tarnamid® T-27 MK30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese CELANEX 2302 GV1/30 PBT, 30% Glass Reinforced
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese CELANEX 3300-2 PBT, 30% Glass Reinforced
Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese Celanex® 6500HF PBT, Mineral / Glass Reinforced
6500HF is a high flow, 30% glass/mineral filled polybutylene terephthalate (PBT) with improved warp resistance and surface smoothness.Information provided by Celanese Corporation.
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 60243-1
Celanese IMPET 2700 GV1/20 PET, 20% Glass Reinforced
Polyethylene terephthalate, 20 % glass fibre reinforced, high flowability, excellent gloss, high modulusInformation provided by Celanese
Dielectric Strength 31.0 kV/mm
787 kV/in
IEC 243-1
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
Dielectric Strength 31.0 kV/mm
787 kV/in
in transformer oil; IEC 60243-1
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft