Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.650 GPa | 94.3 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Tensile Modulus | >= 0.650 GPa | >= 94.3 ksi | 2% sec, TD; ASTM D882 |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | |
Radici Radilon® S 40EP3215 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **) Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | Sintered Molding, DIN 53457 |
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | MD; ASTM D882 |
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a.. |
|||
Tensile Modulus | 0.650 - 0.850 GPa | 94.3 - 123 ksi | MD/TD; ISO 527-3 |
Borealis Bormed™ TD109CF Polypropylene Copolymer Bormed™ TD109CF is a propylene alpha olefin copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: lamination films, food.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | TD; ASTM D882-A |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Tensile Modulus | 0.650 - 0.750 GPa | 94.3 - 109 ksi | ISO 527-3 |
Borealis HD204CF Polypropylene HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru.. |
|||
Tensile Modulus | 0.650 - 0.750 GPa | 94.3 - 109 ksi | MD/TD; ISO 527-3 |
Borealis HD244CF Polypropylene HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr.. |
|||
Tensile Modulus | 0.650 - 0.750 GPa | 94.3 - 109 ksi | MD/TD; ISO 527-3 |
Borealis HD601CF Polypropylene HD601CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: metallisable cast film, inner layer in co extrusion, textile packaging fil.. |
|||
Tensile Modulus | 0.650 - 0.750 GPa | 94.3 - 109 ksi | MD/TD; ISO 527-3 |
Borealis HD621CF Polypropylene HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | |
Covestro Baydur® GS PIR A Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 160 °C |
94.3 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 0.650 GPa @Temperature 160 °C |
94.3 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.650 GPa @Temperature 160 °C |
94.3 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.650 GPa @Temperature 160 °C |
94.3 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12 Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 W 20 PA12 Product Description: Grilamid L 20 W 20 is a semi-flexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 is heat stabilized. The main features of Grilamid L 20.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 23.0 °C |
94.3 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® BM6574 BK316 TPC-ET
(Unverified Data**) Hytrel® BM6574 is a 65 nom. Shore D, plasticiser free high performance resin for blow molding and extrusion; it shows ageing resistance up to 150°C, and excellent mechanical properties at elevated.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 6040IH Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | MD |
BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll Product comes in 2-2.5 mm round pellets.Information provided by BASF |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
3M Dyneon™ TFM™ 1700 Modified PTFE Powder Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera.. |
|||
Tensile Modulus | 0.650 - 0.750 GPa | 94.3 - 109 ksi | MD/TD; ISO 527-3 |
Borealis HD214CF Polypropylene Homopolymer HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus.. |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 0.650 GPa @Temperature 160 °C |
94.3 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
Tensile Modulus | 0.650 GPa | 94.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BM 20 SBG PA* Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features: Lactam freeGood transparency and glossGood flexibility and toughnessVery good ther.. |