Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 12.0 J/cm² | >= 57.1 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Charpy Impact, Notched | >= 12.0 J/cm² | >= 57.1 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m.. |
|||
Charpy Impact, Notched | >= 12.0 J/cm² | >= 57.1 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | EN ISO 179/2 ep b |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S 40EP3215 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 12.0 - 22.0 J/cm² | 57.1 - 105 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO Data, Low Temp |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | Partial; ISO 179/1eA |
DuPont Performance Polymers Hytrel® PC966 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 12.0 J/cm² | 57.1 ft-lb/in² | Partial; ISO 179/1eA |
DuPont Performance Polymers Hytrel® SC969 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature -20.0 °C |
57.1 ft-lb/in² @Temperature -4.00 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® R 60 ES Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A USX200 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |