Polymer Property : Charpy Impact, Notched = 12.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched >= 12.0 J/cm²
>= 57.1 ft-lb/in²
ISO 179
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro..
Charpy Impact, Notched >= 12.0 J/cm²
>= 57.1 ft-lb/in²
ISO 179
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive
Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m..
Charpy Impact, Notched >= 12.0 J/cm²
>= 57.1 ft-lb/in²
ISO 179
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan..
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
EN ISO 179/2 ep b
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite
Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o..
Charpy Impact, Notched 12.0 J/cm²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S 40EP3215 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 12.0 - 22.0 J/cm²
57.1 - 105 ft-lb/in²
DIN 53453
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® BRZ 247 W PA6
Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi..
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a..
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
ISO Data, Low Temp
Dow Prevail® 3050 ABS + Polyurethane
PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
Partial; ISO 179/1eA
DuPont Performance Polymers Hytrel® PC966 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Charpy Impact, Notched 12.0 J/cm²
57.1 ft-lb/in²
Partial; ISO 179/1eA
DuPont Performance Polymers Hytrel® SC969 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Charpy Impact, Notched 12.0 J/cm²

@Temperature -20.0 °C
57.1 ft-lb/in²

@Temperature -4.00 °F
Dry; ISO 179/Af
Arkema Group Orgalloy® R 60 ES Polyamide Alloy
Polyamide Alloy, Film and PackagingInformation provided by Arkema Group
Charpy Impact, Notched 12.0 J/cm²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A USX200 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..