Heatbath/Park #3 Granular Charcoal Pack Carburizing Compound

Category Ceramic , Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park #3 Granular Charcoal Pack Carburizing Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Commonly used in the heat treatment of steel as a pack-hardening medium.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 954 °C
1750 °F
Upper limit of working range
Minimum Service Temperature, Air 816 °C
1500 °F
Lower limit of working range