Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 25.0 - 30.0 MPa | 3630 - 4350 psi | DIN 53 456 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Ball Indentation Hardness | 25.0 - 30.0 MPa | 3630 - 4350 psi | DIN 53 456 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Ball Indentation Hardness | 25.0 MPa | 3630 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
Ball Indentation Hardness | 25.0 MPa | 3630 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Ball Indentation Hardness | 25.0 MPa | 3630 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |