Lanxess Durethan® B 30 S 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant |
Nylon 6, Unreinforced, Flame Retardant |
Durethan®
|
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant |
Nylon 6, Unreinforced, Flame Retardant |
Durethan®
|
Lanxess Durethan® B 30 S FN40 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® B 31 F 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade |
Film |
Durethan®
|
Lanxess Durethan® B 31 SK 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® B 35 FA 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 35 FKA 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 38 FKA 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 40 E 000000 Nylon 6 |
Nylon 6, Extruded |
Durethan®
|
Lanxess Durethan® B 40 F 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 40 FAM 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 40 FKA 000000 Nylon 6, Film Grade |
Nylon 6, Film Grade |
Durethan®
|
Lanxess Durethan® B 40 SK 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® BC 30 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® BC 30 S 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
Durethan®
|
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
Durethan®
|
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
Durethan®
|
Lanxess Durethan® BCF 30 X H2.0 901510 Nylon 6, 30% Glass + Carbon Fiber |
Nylon 6, Carbon Fiber Filled |
Durethan®
|
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres |
Nylon 6, Glass Bead Filled |
Durethan®
|
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced |
Nylon 6, Glass Bead Filled |
Durethan®
|
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 130 CS DUS008 600091 Nylon 6, 30% Glass Fiber |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 135 DUS008 000000 Nylon 6, 35% Glass Fiber |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 140 H2.0 DUS008 900051 Nylon 6, Glass Fiber Reinforced, Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 15 H.3 DUS008 000000 Nylon 6, 15% Glass Fiber |
Nylon 6, 20% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 15 H2.0 901510 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced |
Nylon 6, 20% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers |
Nylon 6, 20% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Durethan®
|
Lanxess Durethan® BKV 20 FN20 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Durethan®
|
Lanxess Durethan® BKV 20 FN20 DUS013 000000 Nylon 6, 20% Glass Fiber |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Durethan®
|
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 215 901510 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers |
Nylon 6, 20% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 215 W1 902176 Copolyamide, 15% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, Glass Filled, Impact Grade |
Durethan®
|
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Durethan®
|
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber |
Nylon 6, 40% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber |
Nylon 6, 40% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced |
Nylon 6, 40% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced |
Nylon 6, 50% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced |
Nylon 6, 50% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber |
Nylon 6, 50% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced |
Nylon 6, 50% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers |
Nylon 6, 50% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced |
Nylon 6, 40% Mineral Filled |
Durethan®
|
Lanxess Durethan® BM 25 FN20 700350 Nylon 6, 25% Mineral |
Nylon 6, 30% Mineral Filled |
Durethan®
|
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral |
Nylon 6, Glass/Mineral Reinforced |
Durethan®
|
Lanxess Durethan® C 38 FA 000000 Copolyamide |
Nylon 6 |
Durethan®
|
Lanxess Durethan® C 38 FKAM 000000 Copolyamide |
Nylon 6 |
Durethan®
|
Lanxess Durethan® C 38 FKS 000000 Copolyamide |
Nylon 6 |
Durethan®
|
Lanxess Durethan® CI 31 F 000000 Copolyamide PA6/6I |
Nylon 6 |
Durethan®
|
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls |
Nylon 6, Glass Bead Filled |
Durethan®
|
Lanxess Durethan® DP 1441/40 H2.0 EF 900116 Nylon 6, 40% Glass Fiber + Mineral |
Nylon 6, Glass/Mineral Reinforced |
Durethan®
|
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Durethan®
|
Lanxess Durethan® DP 1802 H3.0 000000 Nylon 6 |
Nylon 6, Extruded |
Durethan®
|
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Durethan®
|
Lanxess Durethan® DP 2037/30 H2.0 LT 904040 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber |
Nylon 6, 20% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber |
Nylon 6, 20% Glass Fiber Filled |
Durethan®
|
Lanxess Durethan® DP BC 310 EF 000000 Nylon 6 |
Nylon 6, Extruded |
Durethan®
|
Lanxess Durethan® DP BC 310 EF 600065 Nylon 6 |
Nylon 6, Extruded |
Durethan®
|
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6 |
Nylon 6, Unreinforced |
Durethan®
|
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber |
Nylon 6 |
Durethan®
|
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber |
Nylon 6, 30% Glass Fiber Filled |
Durethan®
|