Material Notes:
Copolyamide, film quality, high transparency, with slip agent, not nucleatedApplication Examples: blown film coextrusion (central layer)
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 10 %
10 %
Test Sim. to ISO 62
Moisture Absorption at Equilibrium 3.0 %
3.0 %
23°C/50% R.H.; Test Sim. to ISO 62
Melt Flow 6 g/10 min

@Load 2.16 kg,
Temperature 235 °C
6 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Estimated using room temperature density; ISO 1133
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
10°C/min; ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
Conditioned; IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; IEC 60243-1
Descriptive Properties Value Comments
ISO Shortname ISO 1874-PA 6/IPDI,FS,18-020
Region Asia Pacific
Europe
Near East/Africa
North America
South and Central America