Material Notes:
PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow)
Physical Properties Metric English Comments
Density 1.115 g/cc
0.04028 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0011 cm/cm
0.0011 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527-1/-2
Elongation at Yield 3.8 %
3.8 %
ISO 527-1/-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1/-2
Charpy Impact Unnotched 16.5 J/cm²

@Temperature 23.0 °C
78.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Form Pellets
Processing Injection molding
Other extrusion
Region Asia Pacific
Europe
Near East/Africa
North America
South and Central America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved