Material Notes:
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mold release.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
1.20 g/cc
0.0434 lb/in³
ISO 1183
Water Absorption 0.15 %
<br>@Time 86400 sec
0.15 %
<br>@Time 24.0 hour
ASTM D570
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Moisture Absorption at Equilibrium 0.35 %
0.35 %
ASTM D570
0.58 %
<br>@Temperature 100 °C
0.58 %
<br>@Temperature 212 °F
ASTM D570
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 7.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
7.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
112.2 g/10 min
<br>@Load 5.00 kg,<br> Temperature 300 °C
112.2 g/10 min
<br>@Load 11.0 lb,<br> Temperature 572 °F
ASTM D1238
Melt Index of Compound 7.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
7.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 68.0 MPa
9860 psi
Type I, 50 mm/min; ASTM D638
75.0 MPa
10900 psi
50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527
62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 135 %
135 %
Type I, 50 mm/min; ASTM D638
140 %
140 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527
7.0 %
7.0 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
2.31 GPa
335 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 95.0 MPa
13800 psi
2 mm/min; ISO 178
97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.25 GPa
326 ksi
2 mm/min; ISO 178
2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
1.39 J/cm
<br>@Temperature -30.0 °C
2.60 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 32.04 J/cm
60.02 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
15.0 kJ/m²
<br>@Temperature -30.0 °C
7.14 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.50 J/cm²
35.7 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.50 J/cm²
<br>@Temperature -30.0 °C
7.14 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Tensile Impact Strength 630 kJ/m²
300 ft-lb/in²
Type S; ASTM D1822
Dart Drop, Total Energy 64.0 J
47.2 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
169 J
125 ft-lb
ASTM D3029
65.0 J
<br>@Temperature 23.0 °C
47.9 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
Taber Abrasion, mg/1000 Cycles 10
10
CS-17, 1 kg; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
62.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
34.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
68.4 µm/m-°C
<br>@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
<br>@Temperature -40.0 - 203 °F
ASTM E 831
CTE, linear, Transverse to Flow 57.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
60.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
<br>@Thickness 3.20 mm
275 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
137 °C
<br>@Thickness 6.40 mm
279 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
124 °C
<br>@Thickness 3.20 mm
255 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
132 °C
<br>@Thickness 6.40 mm
270 °F
<br>@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 140 °C
284 °F
Rate B/120; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.96
<br>@Frequency 1.00e+6 Hz
2.96
<br>@Frequency 1.00e+6 Hz
ASTM D150
3.17
<br>@Frequency 50.0 - 60.0 Hz
3.17
<br>@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 14.9 kV/mm
<br>@Thickness 3.20 mm
378 kV/in
<br>@Thickness 0.126 in
in air; ASTM D149
Dissipation Factor 0.00090
<br>@Frequency 50.0 - 60.0 Hz
0.00090
<br>@Frequency 50.0 - 60.0 Hz
ASTM D150
0.010
<br>@Frequency 1.00e+6 Hz
0.010
<br>@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
60 - 120 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
1.00 - 3.15 in/min
UL 746A