Polymer Property : Specific Heat Capacity = 1.25 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific)
Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific)
Nonhalogenated. 17.5 MFR, for small intricate parts.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 123 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific)
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not ..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 124R PC
UL rated HB. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no l..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific)
LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 133 PC
Nonhalogenated. 3.5 MFR. UV-stabilized.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 153R PC
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific)
10.5 MFR. Improved flame retardance. Super mold release.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific)
LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HP2 PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® HPH4504 PPC
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HPS1S PC
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific)
Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades ..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific)
Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® LI1911R PC
Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® ML7678 PC
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East)
LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 144 PC (Asia Pacific)
LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information ..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 144R PC
UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer ..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C 351
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific)
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® 4501 PPC
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HF1140 PC
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
ASTM C351
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
Average value: 1.25 J/g-°C Grade Count:4