Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 17.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 101 PC (Asia Pacific)
Nonhalogenated, 7.0 MFR, for thicker sections without sinks.
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 104 PC
UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will..
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 131 PC
Nonhalogenated. 3.5 MFR.
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 133 PC
Nonhalogenated. 3.5 MFR. UV-stabilized.
Izod Impact, Notched 9.07 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific)
Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 9.07 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 135 PC
General purpose low flow polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific)
7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release.
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release
Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Izod Impact, Notched 9.07 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 134 PC (Asia Pacific)
3.5 MFR. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not be used for medical applicati..
Izod Impact, Notched 9.08 J/cm

@Temperature 22.8 °C
17.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Quantum Polycarbonate
Information provided by Quantum Advanced Engineering Plastics
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade  (discontinued **)
Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui..
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM Data
Styron CALIBREâ„¢ 200 6 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256; ISO 180/4A
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
Izod Impact, Notched 9.07 J/cm
17.0 ft-lb/in
ASTM Data
Styron CALIBREâ„¢ 300 10 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ISO 180/4A
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4310-10 Polycarbonate
EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4330-10 Polycarbonate
EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a..
Izod Impact, Notched 9.10 J/cm

@Temperature 23.0 °C
17.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. ..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
0.125 in; 10 mil notch; ASTM D256
Styron CALIBREâ„¢ 303-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4510-10 Polycarbonate
EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp SBB 3715 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® M Machine Grade Polycarbonate
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Izod Impact, Notched 9.10 J/cm

@Thickness 3.20 mm
17.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se..
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Teknor Apex Sinvicomp SBB 3615 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provide..