Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 339 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 131 PC
Nonhalogenated. 3.5 MFR.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 133 PC
Nonhalogenated. 3.5 MFR. UV-stabilized.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® 221 PC
17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific)
10.5 MFR. Improved flame retardance.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 241R PC
General purpose polycarbonate with 10.5 MFR and internal mold release.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® 955U PC
Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® FXD171R PC (Asia Pacific)
Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.
Flexural Modulus 2.34 GPa
339 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FXG154 PC
FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HPS7R PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® IR2840 PC
7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® LI1813R PC
Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific)
Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® OQ4620R PC
Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® VR2520 PC
General purpose polycarbonate with melt flow rate of 8.5.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 945U PC
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 955 PC
Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 955U PC (Asia Pacific)
Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXE101R PC
Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Hannam Chemical Hanalac 750 ABS, General Purpose
FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect..
Flexural Modulus 2.34 GPa
339 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO
LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
Flexural Modulus 2.34 GPa
<br>@Thickness 3.18 mm
339 ksi
<br>@Thickness 0.125 in
ASTM D790
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Flexural Modulus 2.34 GPa
<br>@Thickness 3.20 mm
339 ksi
<br>@Thickness 0.126 in
Injection Molded; ASTM D790
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color ..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PN275F PPE+PS
PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL 844 PPE+PS (Asia Pacific)
Medium heat PPO/HIPS alloy used in the automotive industry.
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Engineered Plastics EPPC 2014G Polycarbonate
Gray injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation.
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Engineered Plastics EPPC 314C Polycarbonate
Clear; extrusion/blow molding grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation.