Polymer Property : Melt Flow = 7.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® FR15U ABS
Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60).
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific)
Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing.
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific)
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR7020 ASA
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® FXD103 PC
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Melt Flow 7.0 g/10 min

@Load 3.80 kg,
Temperature 200 °C
7.0 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East)
FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East)
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 360 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem 2200N PEI
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 360 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 360 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 680 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ISO 1133
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Techmer ES Plastiblend® ABS 8003 A1
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp..
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Techmer ES Plastiblend® PC/ABS 8800
Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc.
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
from MVR; ISO 1033
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene
Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided..
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis Daplen™ ED206HP TPO Compound
Daplen ED206HP is a 25% mineral reinforced compound intended for injection molding. ED206HP has been developed especially for the car industry, to be used in interior parts requiring excellent scra..
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance..
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Chi Mei Kibiton® PB-585 SBC
Shoe sole industrial accessory
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Total Lacqrene® 740 High Impact Polystyrene  (discontinued **)
LACQRENE® alpha 740 is a high gloss, high impact grade of polystyrene.ApplicationWhite goods (washing machines, driers), Toys and games, Garden equipment, All applications needing high gloss with g..
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific)
ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL.
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East)
GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East ..