Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD103R PC FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | |
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 179 eA |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | |
Ineos ABS Lustran® M203FC Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | |
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 1310 ABS + Polycarbonate PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30 Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BS V0 PA6 Product description: Grilon BS V0 is an unreinforced, normal viscosity, self-extinguishing PA6 injection molding grade. Grilon BS V0 has the following important properties: Halogen and phosphorous-f.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | dry; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROPHEN Polyphenylene ether modified This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include fittings, drive components for domestic appliances, and compon.. |
|||
Charpy Impact, Notched | 1.50 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.50 J/cm² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D.. |