Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D-792
Plaskolite Optix® CA - 51 HF General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Plaskolite Optix® CA-68 General Purpose Acrylic Resin
Injection Molding and Extrusion Grade. Good heat resistance, medium flow.
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 201R PC
7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release.
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer
Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c..
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® EXL1484T PC Copolymer
Lexan* EXL1484T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in c..
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® HPS4 PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable...
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East)
Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope..
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® ML7647 PC
Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region.
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific)
Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D-792
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Density 1.19 - 1.31 g/cc

@Temperature 250 - 250 °C
0.0430 - 0.0473 lb/in³

@Temperature 482 - 482 °F
Average value: 1.25 g/cc Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Density 1.19 - 3.80 g/cc
0.0430 - 0.137 lb/in³
Average value: 1.95 g/cc Grade Count:5
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber  (discontinued **)
Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. ..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific)
LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information..
Density 1.19 g/cc
0.0430 lb/in³
DIN 53.479
Lubrizol Advanced Materials PEARLBOND® 110 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 110 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a low thermoplasticity level.Applications: P..
Density 1.19 - 1.20 g/cc
0.0430 - 0.0434 lb/in³
Average value: 1.20 g/cc Grade Count:17
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Density 1.19 g/cc
0.0430 lb/in³
ISO 2781
Lubrizol Advanced Materials Pearlstick® 45-90/06 Polycaprolactone based TPU
Pearlstick 45-90/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Techmer ES HiFill FR® PC IM FR
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
SABIC Innovative Plastics Noryl GTX LMX171 PPO/PBT (Europe-Africa-Middle East)
Noryl LMX171 is a PPO/PBT blend including conductive agent with a balanced heat/impact property profile. Noryl LMX differentiate from Noryl GTX by a lower moisture uptake (0.15%).This data was suppl..
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Techmer ES Electrablend® PA6/6 03001 Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab..
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183-1-A
BASF Elastollan C 88 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Density 1.19 g/cc
0.0430 lb/in³
Arlon SQA-TMS-024
Arlon R35232B050 0.050" Fully Cured, Static Dissipating Silicone Rubber
Fully cured, unsupported, static dissipating silicone.Design/Construction:Liner: 3 mil PolyethyleneProduct: Fully Cured Silicone RubberCarrier: N/AThis data represents typical values for the produc..
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 290A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Barlog Plastics KEBAFLEX SG 35 A.1 TPE-S, Shore A35, natural
TPE-SInformation provided by BARLOG plastics GmbH.
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® GL3100 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Wanhua Chemical Wanthane® WHT-1580 Polyester Based TPU