| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East)
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 104 PC
UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 104R PC
UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific)
LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 131 PC (Asia Pacific)
Nonhalogenated. 3.5 MFR.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 244R PC
10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 244R PC (Asia Pacific)
LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 4701R PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 4704 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific)
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 920 PC
Opaque colors, low viscosity, superior flame retardance.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific)
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 943A PC
Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Lexan® PPC4701 PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific)
Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 141 PC
General purpose polycarbonate with melt flow rate of 10.5.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific)
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Lexan® HF1140 PC (Asia Pacific)
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors. Effective January 15th, 2007 th..
|
|||
| Hot Wire Ignition, HWI |
30
-
60
sec @Thickness 1.50 mm |
30
-
60
sec @Thickness 0.0591 in |
UL Rating PLC 2 (30-60 sec) |
|
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics ULTEM CRS5201 PEI
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 357 PBT+PC
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Valox® 357U PBT
Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Hot Wire Ignition, HWI |
30
-
60
sec @Thickness 3.00 mm |
30
-
60
sec @Thickness 0.118 in |
UL 746 |
|
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
|
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
|
|||
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
|
SABIC Innovative Plastics Noryl BN30 PPE+PS
Blowmoldable. DTUL 180F. UL rated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Hot Wire Ignition, HWI |
30
-
60
sec @Thickness 3.00 mm |
30
-
60
sec @Thickness 0.118 in |
UL Rating PLC 2 (30-60 sec) |
|
Covestro Makrolon® 3103 Polycarbonate
Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye..
|
|||
| Hot Wire Ignition, HWI |
30
-
60
sec @Thickness 1.10 mm |
30
-
60
sec @Thickness 0.0433 in |
UL Rating PLC 2 (30-60 sec) |
|
Covestro Makrolon® 6465 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici..
|
|||