| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on tensile bar; SABIC Method |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® 134R PC
Nonhalogenated. 3.5 MFR. Internal mold release. FDA food contact compliant in limited colors.
|
|||
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Lexan® 916R PC (Europe-Africa-Middle East)
Lexan* 916R Polycarbonate (PC) resin is a low viscosity, non-filled, injection molding grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating at 0.8 mm properties. Lexan* ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® 923 PC
Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer
18 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HP2R PC
Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® IP300 PC
Improved toughness/impact strength at ambient/low temperatures for automotive instrument panels, knee bolsters and trim. Range gray and black only.This data was supplied by SABIC-IP for the America..
|
|||
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East)
PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0078
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0078
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® 101 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated, 7.0 MFR, for thicker sections without sinks.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 6.40 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.252 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® FL900 PC
Lexan* resin FL900 is a Br- & Cl-free flame retardant grade that can be foamed for weight reductions. UL-94 V1 listed at 3.9mm together with good stiffness, heat, creep and impact performance make i..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
LG Chemical LUPOY GP1000MU PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics PC1003R PC (Europe-Africa-Middle East)
PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Ultem DH1004F PEI
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR
Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
ASTM D955 |
|
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR
Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL PX1265 PPE+PS
Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0080
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific)
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL EM6100 PPE+PS
PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0080
cm/cm <br>@Time 86400 sec
|
0.0050
-
0.0080
in/in <br>@Time 24.0 hour
|
ISO 294 |
|
Eurostar Starflam PW0042E PA6, 20% Mineral Filled, Injection Molded
PW0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Reinforced, Polyamide 6 Injection MoldingInformation provided by Polymer Technology & Services, the North American exclus..
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics PC1803R PC (Europe-Africa-Middle East)
PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Linear Mold Shrinkage, Flow |
0.0050
-
0.0070
cm/cm <br>@Thickness 3.20 mm
|
0.0050
-
0.0070
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics NORYL EN95 PPE+PS (Asia Pacific)
Low heat, extrusion grade PPO/HIPS alloy.
|
|||