| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® 9931X PC (Europe-Africa-Middle East) Lexan* 9931X is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, extreme low temperatu.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® IR2210 PC (Europe-Africa-Middle East) IR2210 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® IR2240 PC (Europe-Africa-Middle East) IR 2240 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific) Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics Lexan® VR2220 PC (Europe-Africa-Middle East) VR2220 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Asia Pacific) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC0703R PC (Europe-Africa-Middle East) PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC1003R PC (Europe-Africa-Middle East) PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East) PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
| Dart Drop, Total Energy | 65.0 J | 47.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics PC1803R PC (Europe-Africa-Middle East) PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||