Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific)
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific)
10.5 MFR. Improved flame retardance.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific)
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific)
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® FXD171R PC (Asia Pacific)
Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® FXG121R PC
PC in special effects colors. ""Diamond Sparkle"" appearance additives. Color package may affect performance.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® FXM121R PC
PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
PLC code 2; UL 746A
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® HPH4704 PPC
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
PLC code 2; UL 746A
SABIC Innovative Plastics Lexan® PPC4704 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral filled PA6 compound
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® 925A PC (Asia Pacific)
Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific)
Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Lexan® HF1110R PC
High flow grade. Easy mold release version of LEXAN HF1110. For thin wall lighting lenses, data storage components and safety eyewear lenses.
Hot Wire Ignition, HWI 30 - 60 sec
<br>@Thickness 1.50 mm
30 - 60 sec
<br>@Thickness 0.0591 in
UL Rating PLC 2 (30-60 sec)
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant &nbsp;(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC
LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
PLC code 2; UL 746A
SABIC Innovative Plastics Valox® 357 PBT
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Hot Wire Ignition, HWI 30 - 60 sec
<br>@Thickness 3.00 mm
30 - 60 sec
<br>@Thickness 0.118 in
UL 746
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific)
ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Valox® 357U PBT+PC
Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific)
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.
Hot Wire Ignition, HWI 30 - 60 sec
<br>@Thickness 3.00 mm
30 - 60 sec
<br>@Thickness 0.118 in
UL 746
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics NORYL BN31 PPE+PS
Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability.
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Hot Wire Ignition, HWI 30 - 60 sec
<br>@Thickness 1.50 mm
30 - 60 sec
<br>@Thickness 0.0591 in
UL Rating PLC 2 (30-60 sec)
Covestro Apec® DP9-9353 High-Heat Polycarbonate, UV Stabilized &nbsp;(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
SABIC Innovative Plastics NORYL PX1005X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications.