| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized |
| Manufacturer | Polymer Technology & Services, LLC (PTS) |
| Trade Name | Tristar® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
| Water Absorption | 0.15 % | 0.15 % | 24 hours at 73°F; ASTM D570 |
| Melt Flow | 8.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 62.1 MPa @Thickness 3.17 mm |
9010 psi @Thickness 0.125 in |
ASTM D638 |
| Elongation at Break | 130 % @Thickness 3.17 mm |
130 % @Thickness 0.125 in |
ASTM D638 |
| Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
| Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
| Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
| 137 °C | 279 °F | ISO 75 | |
| UL RTI, Electrical | 125 °C | 257 °F | |
| UL RTI, Mechanical with Impact | 115 °C | 239 °F | |
| UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
| Flammability, UL94 | V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
|
| Glow Wire Test | 775 °C | 1430 °F | GWIT |
| 960 °C | 1760 °F | GWFI |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | PLC 2 |
| Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
| 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 | |
| High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
| >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
PLC 0 | |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | PLC 3 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 277 - 291 °C | 530 - 555 °F | |
| Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
| Front Barrel Temperature | 299 - 318 °C | 570 - 605 °F | |
| Nozzle Temperature | 291 - 318 °C | 555 - 605 °F | |
| Melt Temperature | 302 - 329 °C | 575 - 625 °F | |
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
| Drying Temperature | 121 °C | 250 °F | |
| Dry Time | 3 - 4 hour | 3 - 4 hour | 48 hours max. |
| Injection Pressure | 96.5 - 138 MPa | 14000 - 20000 psi | |
| Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
| Clamp Pressure | 27.6 - 68.9 MPa | 4000 - 10000 psi | |
| Shot Size | 40 - 60 % | 40 - 60 % | |
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Injection Speed- Edge Gate | Slow to Medium | |
| Injection Speed- Tab Gate | Medium to Fast | |
| Injection Speed- Tunnel Gate | Fast |