Polymer Property : Flexural Modulus = 2.21 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
Tangent; ASTM D790
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black
Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Omni Plastics OmniLon™ 6/6 PA6/6 IM8 Unfilled/ Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources ABS-FR1 ABS, Flame Retardant
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow
Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Flexural Modulus 2.21 GPa
<br>@Thickness 3.17 mm
321 ksi
<br>@Thickness 0.125 in
ASTM D790
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.21 GPa
321 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Flexural Modulus 2.21 GPa
321 ksi
ASTM D790
PolyOne Maxxam™ 34-1520 Silver Metallic TFPP Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 2.21 GPa
321 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Flexural Modulus 2.21 GPa
<br>@Thickness 3.17 mm
321 ksi
<br>@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.21 GPa
<br>@Thickness 3.17 mm
321 ksi
<br>@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.21 GPa
<br>@Thickness 3.17 mm
321 ksi
<br>@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.21 GPa
321 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa..
Flexural Modulus 2.21 GPa
<br>@Temperature 23.0 °C
320 ksi
<br>@Temperature 73.4 °F
ASTM D790
IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene
Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets
Flexural Modulus 2.21 GPa
321 ksi
Kraton® G1650 + PP blend + Talc (12/21/67)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Flexural Modulus 2.21 GPa
321 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal
LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman 310 Utility Black PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Flexural Modulus 2.21 - 2.62 GPa
320 - 380 ksi
ASTM D790
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Flexural Modulus 2.21 GPa
321 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific)
PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack..
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Clariant Renol PA2SP0017 Nylon 6, Impact Modified
Data provided by Clariant Masterbatches
Flexural Modulus 2.21 GPa
<br>@Thickness 6.40 mm
320 ksi
<br>@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AP-78 EP ABS Electro Plating Applications
Electroplating & Hot Stamping GradesInformation provided by Bhansali
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Aaron Industries AAROPRENE® GFIPP 2010 High Impact Glass Filled Polypropylene
AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 2.21 GPa
<br>@Thickness 6.40 mm
320 ksi
<br>@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade
Electroplating, High FlowInformation provided by Bhansali
Flexural Modulus 2.21 GPa
320 ksi
Zylog Hipolyene® 8021 MF HF Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 2.21 GPa
321 ksi
ASTM D790
Eastman Tenite Acetate 109E3V36324 Clear, Trsp Cellulose Acetate &nbsp;(discontinued **)
Plasticizer 24%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..