Polymer Property : Clamp Pressure = 10000 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer  (discontinued **)
A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Vyram™ 9103-54 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Vyram™ 9203-54 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 41.0 - 69.0 MPa
5950 - 10000 psi
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide..
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Samyang Trirex® PC-3020HF 22 MFI Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
Clamp Pressure 41.0 - 69.0 MPa
5950 - 10000 psi
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Clamp Pressure 41.0 - 69.0 MPa
5950 - 10000 psi
LNP ULTEM® SMU5835 Polyetherimide, 25% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..