| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products G13P100-589UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (YR169L) Mild Beige
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products HP521-187 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9779 Medium Grey
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
|
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
|
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products HP516-01 7% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trimCenter consolesHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
|
RheTech Products HP525-01 30% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Center consolesInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
|
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.345 MPa | 50.0 psi | |
|
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
LNP Stat-Kon® EC-1008 EM BK8-115 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **)
Features: Electrically Conductive, Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
LTL Color Compounds ColorFast® FRA203 ABS
Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
LTL Color Compounds ColorFast® NY2115 Nylon 66
Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
LTL Color Compounds ColorFast® PBA1000 PBT/ABS Alloy
PBT/ABS alloy with excellent physical properties and chemical resistanceAll information provided by LTL Color Compounders, Inc.
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy
Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati..
|
|||
| Back Pressure | 0.345 MPa | 50.0 psi | |
|
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good..
|
|||
| Back Pressure | 0.345 MPa | 50.0 psi | |
|
Multibase Multi-Flex® A 7455 ER TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
|
|||
| Back Pressure | 0.345 MPa | 50.0 psi | |
|
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Back Pressure | 0.345 MPa | 50.0 psi | |
|
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
|
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
|
Clariant Renol PBTSP0006 Polyester Elastomer
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.345 - 0.827 MPa | 50.0 - 120 psi | |
|
Clariant Renol BR7039G15 Nylon 6, 15% Glass Fiber, bondable to TPU
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **)
Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||