Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 960 °C | 1760 °F | at 3 mm |
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
Flammability Index; IEC 60695-2-12 |
PolyOne OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-1 |
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 695-2-1 |
Polykemi AB POLYblend 83FR PC/ABS-Blend, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CY201 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY201 is an industrial quality PC+ABS Flame Retardant grade for injection moulding applications. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CY203 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY203 is a industrial quality PC+ABS flame retardant grade for injection moulding applications. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
Glow Wire Test | 960 °C | 1760 °F | GWFI |
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics ULTEM 2110 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL ENV150 PPE (Europe-Africa-Middle East) Noryl* ENV150 modified polyphenylene ether resin is an unfilled, flame retardant high heat grade suitable for extrusion molding conversion route. It uses non-chlorinated, non-brominated FR additives.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
Cossa Polimeri ESTAPROP 1040 T8 V0 Flame Retardant Polypropylene Flame retardant class V0, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
Cossa Polimeri ESTAPROP 1040 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 960 °C | 1760 °F | CEI 60695/2/1 |
Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
plaque; IEC 60695 |
Eurotec® Tecomid® NB40 NL FA 50 PA 6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |