Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | thick wall - thin wall |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 71.0 - 104 °C | 160 - 219 °F | |
Styron EMERGEâ„¢ 4530-15 Polycarbonate EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Mold Temperature | 82.0 - 104 °C | 180 - 219 °F | |
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |