Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 68.9 MPa
4000 - 10000 psi
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer
SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5..
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC SunPro® SP 200 P3081 Polypropylene Copolymer
SunPro® SP 200 P 3081 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM PP ..
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC X-PRO CTC PP 5002 Polypropylene Copolymer
X-PRO PP 5002 is a polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer
X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC).
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC X-PRO PP 2050 Polypropylene Copolymer
X-PRO PP 2050 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC X-PRO TF 1020 GP Polypropylene Homopolymer, 20% Talc Filled
X-PRO TF 1020 GP is a 20% talc reinforced polypropylene homopolymer. It has applications in general purpose industrial, automotive, consumer, and construction.Data provided by Composite Technologies..
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled
X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden produc..
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled
X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn ..