| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E831-06 |
| PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C | 39.0 µin/in-°F | ASTM D696 |
| Techmer ES Electrablend® PA6/6 C14 BK 14% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C | 39.0 µin/in-°F | ASTM D696 |
| Techmer ES HiFill FR® ASA FR-2A WT209 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant, Good Toughness and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C | 39.0 µin/in-°F | ASTM D696 |
| Techmer ES HiFill FR® PA6/6 FR 344 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C | 39.0 µin/in-°F | ASTM D696 |
| Techmer ES HiFill® ASA 778 UV WT168 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C | 39.0 µin/in-°F | ASTM D696 |
| Techmer ES Plastiblend® TPX-HTN-000BB Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
| CTE, linear, Parallel to Flow | 70.2 µm/m-°C | 39.0 µin/in-°F | ASTM D696 |
| Techmer ES HiFill FR® PA6/6 FR 344 BK Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||